abstract |
Aromatic polyetherketones and polyether sulphones are prepared from a hydrated alkali metal bisphenate by heating a substantially equimolar mixture of the bisphenate and an activated aromatic dihalide in the presence of an aromatic sulphone to distil off the water, preferably at atmospheric pressure, and then heating at temperatures in the range 250° to 400° C. to effect polymerization. |