abstract |
New chelate exchange resins capable of selective recovery of copper, nickel, and other valuable metals from an acidic aqueous leach liquor are prepared by reacting a crosslinked haloalkyl polymer matrix resin (I) with certain aminopyridines (II) to give a resin (III) ##STR1## with pendent methyleneaminopyridine groups attached to the matrix resin. Particularly useful resins are obtained by reacting chloromethylated styrene-divinylbenzene copolymer beads with an aminomethylpyridine, such as 2-picolylamine, N-methyl-2-picolylamine, N-(2-hydroxyethyl)-2-picolylamine, N-(2-methylaminoethyl)-2-picolylamine, or bis-(2-picolyl)amine. At a typical copper ore leach liquor pH of about 2, the picolylamine resins will absorb 15-30 mg copper/ml resin with a 5-10 fold selectivity for copper over ferric iron. |