Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a22da5b7dd6ed60a21538e5edb23e051 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L25-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 |
filingDate |
1976-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1978-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dd5028aa8dfc4e8b5fbae737987652b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7508b88cc22ce9f7fa8163c16f6dffca |
publicationDate |
1978-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4069288-A |
titleOfInvention |
Method for preparing fire retardant molding compositions |
abstract |
Disclosed herein is a method for preparing fire retardant styrenic polymer molding compositions with improved impact strength which compositions contain a metal oxide and a halogenated fire retardant additive. The method comprises dispersing the metal oxide into a minor portion of the styrene polymer component using high intensity mixing and temperatures at or above the fusion temperature of the styrene polymer in order to obtain a uniform dispersion. The metal oxide-polystyrene dispersion is then blended with the other ingredients of the polyblend. The resulting blend is compounded at temperatures greater than 255 DEG C. and then comminuted to form a molding composition. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7504451-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7528191-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5516814-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2008004381-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6239197-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006155035-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4395511-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006155018-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4530880-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5171757-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5059650-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5053444-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4543281-A |
priorityDate |
1976-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |