Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b3853d6ee291379ca9a3a346d61c9b4f |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E21B36-003 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21B36-00 |
filingDate |
1976-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1977-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_439dbab88f6fd1e390162ac8b8043477 |
publicationDate |
1977-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4024919-A |
titleOfInvention |
Technique for insulating a wellbore with silicate foam |
abstract |
Disclosed herein is a method for thermally insulating a well. The well is insulated by boiling a solution containing silicate in contact with well tubing to form a coating of silicate on the tubing. A fluid substantially free of silicate also contacts the well tubing to buffer a lower portion of the tubing from the silicate solution. This substantially silicate-free fluid prevents silicate foam coating on the lower portion of the tubing and thus alleviates problems associated with having silicate foam coated thereon. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0045099-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6085839-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7410013-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0045099-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5297627-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6336408-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6536526-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4693313-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2004144566-A1 |
priorityDate |
1976-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |