Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_782b276beee7c34efe50183392517dfb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-30 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22C3-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C3-00 |
filingDate |
1975-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1977-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_495f2125efceb9ff3bfa44dbabbe4abb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65f245128c62b0b44df1ecf3802c6130 |
publicationDate |
1977-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-4002784-A |
titleOfInvention |
Coating method for graphite |
abstract |
A method of limiting carbon contamination from graphite ware used in induction melting of uranium alloys is provided comprising coating the graphite surface with a suspension of Y2O3 particles in water containing about 1.5 to 4% by weight sodium carboxymethylcellulose. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0427392-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-0427392-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4500602-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2797990-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2783778-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5221336-A |
priorityDate |
1975-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |