Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_990a6ea5cab2e817262cb26a0c6175d5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-584 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C253-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-92 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C255-49 |
filingDate |
1975-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1976-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63e0bbe8e95c5f99e92ce11f30e6f66d |
publicationDate |
1976-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-3987080-A |
titleOfInvention |
Regeneration of vanadium-bronze ammoxidation catalyst |
abstract |
In an ammoxidation system where hydrocarbon, oxygen and ammonia are reacted at a temperature of from about 375°C. to about 450°C. in the presence of a vanadium bronze catalyst, the improvement of regenerating heat damaged catalyst by cooling the catalyst to below about 400°C. and then reheating it to a temperature of from about 510°C. to about 530°C. in the presence of oxygen. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5214912-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5216875-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4893465-A |
priorityDate |
1975-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |