Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8efbae6056f7ee0275c50b0f1e7243be |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2375-08 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0095 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-302 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-00 |
filingDate |
1974-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1975-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e912257d5488f33dc34e79e2675ba6ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d7f1abebb4343da9bc95b4c6b30034b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1d133291d6d3218cf837a70d0abc0bc |
publicationDate |
1975-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-3910858-A |
titleOfInvention |
Novel process and product |
abstract |
Structural discontinuities, commonly referred to as splits and voids, which are prevalent in flexible and semiflexible polyurethane foams that have been rendered flame resistant using halogen-containing polymers in combination with antimony oxide are eliminated by the use of barium carbonate. |