Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3e9445e5e3626f36e932c6451a928250 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K2240-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B27K3-15 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F9-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F9-5407 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-431 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M15-667 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-673 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-667 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-431 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F9-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27K3-15 |
filingDate |
1972-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1975-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e093fd9b75520864045588e7205f41cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dd3f33eccae8c8115453b753f932449 |
publicationDate |
1975-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-3878245-A |
titleOfInvention |
Process for the manufacture of phosphorus-containing condensation products, the products and their use as flameproofing agents |
abstract |
The subject of the invention is a process for the manufacture of water-soluble condensation products of hydroxymethyl-phosphonium compounds, characterised in that (a) 1 mol of a tetrakis(hydroxymethyl)-phosphonium compound is condensed with (b) 0.02 to 0.2 mol, preferably 0.05 to 0.15 mol, of urea at 40* to 120*C and optionally in the presence of an inert organic solvent and if appropriate free hydroxyl groups are at least partially etherified with at least one alkanol with 1 to 4 carbon atoms and if appropriate the salts of the condensation products are converted into the corresponding hydroxides. The condensation products are used for flameproofing organic fibre material, especially textiles. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4067927-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4228100-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-3994971-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4311855-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5320785-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4045173-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4806620-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4095945-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4784918-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6541068-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-3002729-A1 |
priorityDate |
1971-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |