Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5c24684033fba97d1ad845ce453a57e3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-688 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-688 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 |
filingDate |
1969-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1972-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a93ce059c7a2d8594f0e3f453a1dd8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_280ab366eba18441648930deced8b092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_419594565371d2ba6738e4f9bc9dbf35 |
publicationDate |
1972-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-3655844-A |
titleOfInvention |
Process for the manufacture of shaped structures with improved dye affinity |
abstract |
IN THE MANUFACTURE OF COPOLYESTERS FROM TEREPHTHALIC ACID OR THE LOW MOLECULAR WEIGHT ALKYL ESTERS THEREOF AND ETHYLENE GLYCOL, DEFINITE MERCAPTALS AND/OR THIOKETALS ARE INCORPORATED INTO THE MACROMOLECULE BY ESTER LINKAGE. THE POLYESTERS ARE SHAPED FROM THE MELT AND SULFONIC ACID GROUPS ARE PRODUCED IN THE SHAPED STRUCTURES BY AN OXIDATIVE AFTER-TREATMENT. THE STRUCTURES HAVE A HIGH AFFINITY FOR CATIONIC SUBSTANCES. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5670657-A |
priorityDate |
1966-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |