Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0decf09d68321711546ec121dd6665c3 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22F1-08 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22F1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-02 |
filingDate |
1969-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1971-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_233fefc6261dc14ef70d183f95d34061 |
publicationDate |
1971-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-3595705-A |
titleOfInvention |
Copper-boron-sulfur alloy and method of treatment |
abstract |
A COPPER BORON SULFUR ALLOY CONTAINING MINOR AMOUNTS OF BORON AND SULFUR IS PROVIDED BY THIS INVENTION. WHEN THIS HIGH CONDCUTIVITY ALLOY IS SOLUTION ANNEALED, RAPIDLY COOLED TO ROOM TEMPERATURE AND SUBSEQUENTLY COLD WORKED, IT HAS A HIGH SOFTENING TEMPERATURE. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-4118256-A |
priorityDate |
1969-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |