abstract |
A polyolefin composition obtainable by blending a) 96.0 to 99.7 wt.-% of a blend (A), being a recycled material comprising A-1) 30 to 70 wt.-% isotactic polypropylene homopolymer, A-2) 20 to 50 wt.-% polyethylene and ethylene containing copolymers, A-3) 0.5 to 4.0 wt.-% polyamide-6,various optional components, A-11) 1 ppm to 100 ppm of limonene, and A-12) 1 ppm to 200 ppm total fatty acid content with a maleic anhydride-grafted SEBS block copolymer, characterized by its melt volume rate and maleic anhydride content. |