http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2022267599-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0869 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L77-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 |
filingDate | 2020-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fdd189f6ec92932c4f715bc3a7bfdb3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_771c42803c7ca2d402b153d5b507f44b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4c30940ab7b561c494c685932bdaac86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ddf3faf10f8f5bee72067e5ed352c60 |
publicationDate | 2022-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2022267599-A1 |
titleOfInvention | Resin composition and resin molded article made of the resin composition |
abstract | A resin composition includes a polyolefin resin (a) and a polyamide resin (b) accounting for 100 wt % in total, the polyolefin resin (a) and the polyamide resin (b) accounting for 70 to 30 wt % and 30 to 70 wt %, respectively, and a surface of a molded resin product produced from the resin composition, analyzed by infrared microspectrometry, giving a spectrum peak intensity ratio of 3.0 to 5.0 as calculated by equation (1), wherein a melt viscosity ratio defined by equation (2) is 0.35 to 0.64 when measured at a shear rate of 1.216 second −1 and at a temperature of Tp+20° C., wherein Tp (° C.) represents the melting point of the polyolefin resin (a) or that of the polyamide resin (b), whichever is higher: n n n n n n n n n Peak n n n intensity n n n ratio n n = n n n absorbance n n n near n n n 2 n n , n TagBox[",", "NumberComma", Rule[SyntaxForm, "0"]] n n 950 n n n n cm n n - n 1 n n n n n absorbance n n n near n n n 3 n n , n TagBox[",", "NumberComma", Rule[SyntaxForm, "0"]] n n 300 n n n n cm n n - n 1 n n n n n n n n n ( n 1 n ) n n n n n n n n Melt n n n viscosity n n n ratio n n = n n n n melt n n n viscosity n n n of n n n polyamide n n n resin n n n n ( n b n ) n n n n melt n n n viscosity n n n of n n n polyolefin n n n resin n n n n ( n a n ) n n n n . n n n n n n ( n 2 n ) |