Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b657bae7c6ba14f228fefd2393ecc834 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C2204-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C21-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C4-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C3-095 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C4-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C3-083 |
filingDate |
2021-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bf876f3c32e1d7d0b229b4fc033bfba0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a22a8b64db4f315b0e749a668136076 |
publicationDate |
2022-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2022033299-A1 |
titleOfInvention |
Chemically strengthened glass, and method for manufacturing the same |
abstract |
The present invention relates to a chemically strengthened glass having a thickness of t [mm], and having a profile of a stress value CS x [MPa] at a depth x [μm] from a surface of the glass, the stress value being measured by a scattered-light photoelastic stress meter, in which a second-order differential value CS x ″ of the stress value CS x in the profile satisfies the following expression within a range of CS x ≥0: 0<CS x ″≤0.050. |