Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bc905cbef116a1ec61d12125af9427f3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L2300-216 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-0015 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-0042 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-043 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-0036 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L24-0089 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L24-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L24-04 |
filingDate |
2021-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d107facc2908e8c4d1019a8a584dbcbf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f37e3b821df1dded0edf491c4d42567d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13e6ad78946bedcca491e815c3884e55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2e1c08c9f681b474e0794108c7dd60c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_644a775b4b09ea20a2e5c7dcea693660 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d785cde9b26ea120b615764f656a4884 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81c8401eeef307076d7436434e1039ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_441649d21dc8467cff86526a5821abb8 |
publicationDate |
2021-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2021322625-A1 |
titleOfInvention |
Non-fibrous porous film and method for tissue adhesion |
abstract |
The present disclosure provides a method for manufacturing a porous film, including: preparing a polymer mixture solution, wherein the polymer mixture solution includes polycaprolactone and at least one hydrophobic polymer; adding solid particles as a dispersing agent to the polymer mixture solution and mixing the solid particles with the polymer mixture solution, wherein the amount of solid particles added is enough to convert the polymer mixture solution into a solid mixture; drying the solid mixture to form a film; and washing the film with a washing fluid to remove the solid particles from the film to form the porous film, wherein the weight ratio of the polycaprolactone to the at least one hydrophobic polymer is about 1:0.1-10, and wherein the weight ratio of the polycaprolactone and the at least one hydrophobic polymer to the solid particles is about 1:0.01-250. |