abstract |
A preparation method comprises following steps: S1: dissolving a coupling agent in an ethanol solution, adding an ultrafine radiopaque agent powder in the ethanol solution, and obtaining a modified ultrafine radiopaque agent powder by agitation, washing and drying, the ultrafine radiopaque agent powder having a particle size of 0.35-0.8 μm; S2: obtaining the radiopaque material by mixing a medical polymeric material with the modified ultrafine radiopaque agent powder. A prepared radiopaque material exhibits not only radiopaque functions but also good mechanical properties of improved elastic modulus, fracture strength and bending modulus, thereby expanding application of medical polymer hollow fibers in high-end medical products for minimally invasive intervention. Particularly, delivery devices applied with prepared radiopaque material have improved pushing and torque performance and are suitable for ultra-smooth guidewires, heart valve prostheses, guiding catheters, and degradable balloons. |