abstract |
To provide a decorative film whereby cracking is suppressed when the decorative film is adhered to a three-dimensional molded product while it is being stretched or in a stretched state. To further provide a composition, a method for producing the decorative film, and a method for producing a three-dimensional molded product provided with the decorative film. The decorative film has at least a base film and a fluororesin layer containing a fluororesin having a crosslinked structure, characterized in that the fluororesin layer contains a urethane bond and an allophanate bond, and the average molecular weight between crosslinking-points of the fluororesin layer is more than 50,000 and at most 100,000. |