abstract |
Provided are a laminate having excellent appearance such as tint and excellent light transmittance, a composite, and a method for producing a composite. The laminate includes a metal foil having a plurality of through-holes penetrating therethrough in a thickness direction, and a positive photosensitive resin layer provided on at least one surface of the metal foil, in which, in the metal foil, an average opening diameter of the through-holes is 0.1 to 100 μm and an average opening ratio determined by the through-holes is 0.1% to 90%. The composite includes a laminate, in which the positive photosensitive resin layer has a plurality of through-holes penetrating therethrough in a thickness direction, the average opening diameter of the through-holes is 0.1 to 100 μm, and the average opening ratio of the through-holes is 0.1% to 90%. |