Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1dbdbd42540fa9bcc9b547f9918dd672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fb823e72d0004ded507f810e2db46fb5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-346 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5419 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-346 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B7-295 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-307 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-441 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-02 |
filingDate |
2020-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_348c44dd8abfb95ed4ab567afb0fce5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7442be7c218d297a46ecd9c8aa7c63cc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1774aee32c748cd2ed19bb4db31b167a |
publicationDate |
2020-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2020303088-A1 |
titleOfInvention |
Flame retardant electrical cable |
abstract |
A flame-retardant electric cable has a core including an electric conductor and an electrically insulating layer. The electrically insulating layer includes a flame-retardant polyolefin-based composition which includes, as base polymer, a mixture of at least two polyolefin homopolymers and/or copolymer wherein at least one is a low-density polyethylene copolymer having a density lower than 0.915 g/cm3. The flame-retardant polyolefin-based composition also includes calcinated kaolin in an amount greater than 3 phr, a metal hydroxide in an amount greater than 10 phr, and an alkyl or alkenyl alkoxy siloxane. The alkyl or alkenyl alkoxy siloxane is in an amount ratio of from 1:25 to 1:50 with respect to the sum of the amounts of calcinated kaolin and of the metal hydroxide. |