Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e164bcc4bd54075650f89b687ea057ff |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D2101-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D2203-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D2101-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D2101-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B34-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A62D3-37 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B34-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D3-37 |
filingDate |
2020-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2e9ce1b83b71a609116ca0b7e4a65a2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8129a96781e16342a760f90415e2445b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6028fcee2e4dd7838fb04711af4245a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b76b8da3e77551d1fd3cbbf7ff5b2e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f4a6c38c1428e238e7e7471f1e2afbe |
publicationDate |
2020-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2020282252-A1 |
titleOfInvention |
Method For Detoxifying Chromium Slag By Using High Sulfur Coal |
abstract |
The present invention discloses a method for detoxifying chromium slag by using high sulfur coal. The method includes: sieving chromium slag into coarse-grained chromium slag and fine-grained chromium slag, air-drying and crushing both the coarse-grained chromium slag and the fine-grained chromium slag; separately mixing the crushed coarse-grained chromium slag and fine-grained chromium slag with the crushed high sulfur coal uniformly; adjusting pH values of a coarse-grained slag mixture and a fine-grained slag mixture to 8.0-11.0 and moisture content thereof to 12%-18%; conducting reduction on the treated coarse-grained slag mixture and fine-grained slag mixture, where the reduction temperature of the fine-grained slag mixture is 500-700° C., the reduction time of the fine-grained slag mixture is 10-30 min, the reduction temperature of the coarse-grained slag mixture is 800-1000° C., the reduction time of the coarse-grained slag mixture is 10-30 min; after the reduction, conducting water quenching, and discharging the product. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114652995-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114717371-A |
priorityDate |
2019-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |