Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61B5-291 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61B5-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-24 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-22 |
filingDate |
2018-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fe7ff741f60388176cac4ec0b3429562 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f7e43ffaea57e5eb01295c9fcc67454 |
publicationDate |
2020-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2020258655-A1 |
titleOfInvention |
Conductive paste, stretchable conductor and electronic component using same, and clothes-type electronic device |
abstract |
A stretchable conductor forming paste containing a conductive filler, a polyurethane elastomer having a glass transition temperature (Tg) of −60° C. to −10° C. and a urethane group concentration of 3000 to 4500 m equivalent/kg, and an organic solvent. Preferably, a total amount of components excluding the solvent is 100 parts by mass, a total of the conductive filler is 70 to 95 parts by mass, and an amount of the polyurethane elastomer is 5 to 30 parts by mass. The obtained paste is printed or coated and then dried to obtain a stretchable conductor, capable of forming a wiring line having good repeated stretchability. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11629455-B2 |
priorityDate |
2017-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |