abstract |
heating the oxygen-absorbing multilayer body which has been irradiated with radiation in the sterilizing step at a temperature of the glass transition temperature of the thermoplastic resin (a) minus 20° C. or more and lower than the glass transition temperature of the thermoplastic resin (a) for 50 hours or more. |