abstract |
A process for hydrocracking 2,4-dimethylpentane and/or 2,2,3-trimethylbutane can comprise: contacting a hydrocracking feed stream in the presence of hydrogen with a hydrocracking catalyst, wherein the hydrocracking feed stream comprises at least 0.5 wt % of 2,4-dimethylpentane and/or 2,2,3-trimethylbutane, based upon a total weight of the hydrocracking feed stream; and wherein the hydrocracking catalyst comprises a medium pore zeolite having a pore size of 5-6 A and a silica to alumina molar ratio of 20-75; preferably the hydrocracking catalyst comprises a medium pore zeolite having a pore size of 5-6 A and a silica to alumina molar ratio of 20-75 and a large pore zeolite having a pore size of 6-8 A and a silica to alumina molar ratio of 10-80, wherein the hydrogenation metal is deposited on the medium pore zeolite and the large pore zeolite. |