Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5f7f120efe096284c7389702c969cf3d |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-418 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2457-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2307-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133334 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F2202-22 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-3025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-208 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-136204 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133528 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2016-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1198845cf4050d6b0c229b941a170ac6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_992aa196018d76a3194d5c01756ee1d3 |
publicationDate |
2018-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2018356565-A1 |
titleOfInvention |
Antistatic film, manufacturing method therefor, polarizing plate and liquid crystal display device |
abstract |
An antistatic film including: a substrate film layer formed of a thermoplastic resin containing a polymer containing an alicyclic structure; and an antistatic layer containing metal oxide particles having electroconductivity, the antistatic layer being provided on the substrate film layer, wherein the antistatic layer has a surface resistance of 1.0×10 6 Ω/square or more and 1.0×10 10 Ω/square or less, and image clarity of a surface of the antistatic layer is 90 or more. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11216127-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11256129-B2 |
priorityDate |
2015-06-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |