abstract |
Disclosed herein are a modifier having a continuous phase (A) containing a second polyolefin resin and a dispersed phase (B) containing a polyamide resin and a modified elastomer, wherein the dispersed phase (B) is composed of a melt-kneaded product of the polyamide resin and the modified elastomer having a reactive group, and wherein when a total of the continuous phase (A) and the dispersed phase (B) is 100% by mass, a content of the dispersed phase (B) is 80% by mass or less, a method for using the modifier, including mixing 0.5 parts by mass or more but 70 parts by mass or less of the modifier per 100 parts by mass of a first polyolefin resin, and a method for producing the modifier, including the step of melt-kneading the second polyolefin resin and a melt-kneaded product of the polyamide resin and the modified elastomer. |