http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018291241-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_26c475bcbe0c24b485b6f37c45cd921f |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2037-1215 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L15-585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J153-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-1207 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J153-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-12 |
filingDate | 2018-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a71170410d44d74e8f809996c720d192 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a92573736041eda27ed7d5c244dac2e2 |
publicationDate | 2018-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2018291241-A1 |
titleOfInvention | Hot-melt adhesive agent |
abstract | Problem to be solved of the present invention is to provide a hot-melt adhesive agent which is capable of applying at low temperature, excellent in adhesiveness at the wide temperature ranges (10 to 40° C.), and excellent in balance between tackiness and retention force, and a disposable product obtained by employing the hot-melt adhesive agent. Means for Solving the problem is a hot-melt adhesive agent comprising a thermoplastic block copolymer (A) which is a copolymer of vinyl class aromatic hydrocarbons and conjugated diene compounds, wherein the thermoplastic block copolymer (A) comprises the following component (A1) and component (A2): (A1) a radial type styrene block copolymer having a styrene content of 35 to 45% by weight, a diblock content of 50 to 90% by weight, and has a viscosity at 25° C. as 25% toluene solution of not more than 250 mPa·s; and (A2) a triblock type styrene block copolymer. |
priorityDate | 2013-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links