abstract |
A method for producing a porous body, comprising a raw-material mixing step of mixing talc having an average particle size of 1 μm or more and 18 μm or less, alumina, an auxiliary raw material containing a material that undergoes a eutectic reaction with talc and being prepared in an amount so as to satisfy a weight ratio of 0.5% or more and 1.5% or less by weight relative to the talc, and a pore-forming agent, to provide green body, and a molding and firing step of molding the green body to provide a compact and firing this compact at a firing temperature of 1350° C. to 1440° C. |