abstract |
A method for forming a cell of a lithium-ion battery comprising a material for a positive electrode having a pore ratio of between 20 and 35% and comprising at least one sacrificial salt, a material for a negative electrode, a separator and an electrolyte, comprising the following successive steps: (a) heating the cell to a temperature T of between 30 and 45° C.; and (b) charging the cell to a potential lower than or equal to 4.8 V, preferably between 4.6 and 4.8 V, even more preferably between 4.7 and 4.8 V. |