http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017335275-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_74b749911ec18eda744e27e76d1e6603
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12R2001-01
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12R1-01
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12N1-205
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12N1-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B3-44
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0071
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C12N1-00
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12R1-01
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N1-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B15-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B3-18
filingDate 2015-08-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d37fa966b235f336a17ee607e29132ec
publicationDate 2017-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2017335275-A1
titleOfInvention Copper sulphide leaching in ferrous chloride medium with bacteria
abstract A method for leaching secondary and primary sulphides of copper in a ferrous chloride medium with iron-oxidising bacteria adapted from the crushing of the mineral from the mine, includes steps of: mixing the mineral from the crushing with concentrated sulphuric acid; transporting the material mixed with sulphuric acid by means of a belt; adding a liquid leaching solution at an intermediate point during transport on the belt, the solution consisting of: iron (II) sulphate to reduce the redox potential of the solution-mineral mixture to values less than 550 mV Ag/AgCl; iron (III) sulphate; bacteria and archaea of the mesophile- and thermophile-type belonging to the genera Acidithiobacillus, Leptospirillum and Sulfulobos; and sodium chloride to produce a chlorinated environment in solutions. The method also comprises the subsequent steps of: heaping the material on heap pads; during the resting step, injecting air warmed by a liquid/air exchange system; and leaching the heaped material.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112074618-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021032723-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019193403-A1
priorityDate 2014-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2002194962-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID227480664
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID66966294

Total number of triples: 29.