Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f8877d26e7e712d48efb03a75bd073f3 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2367-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-003 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-092 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E21B33-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E21B41-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21B33-12 |
filingDate |
2015-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1eb821d59a07515a6075675fb1151548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_be0e00650e1b617d12035365b65534c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e5e69d1e173dcac9eaa2fb4251f86db4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5783b115044a324a94910ac688b438a |
publicationDate |
2017-06-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2017175481-A1 |
titleOfInvention |
MOLDED PRODUCT HAVING EFFECTIVE THICKNESS OF 1 mm OR MORE AND CONTAINING ALIPHATIC POLYESTER RESIN, AND DOWNHOLE TOOL MEMBER FOR HYDROCARBON RESOURCE RECOVERY |
abstract |
Provided are a molded product having an effective thickness of 1 mm or more, the molded product being formed from an aliphatic polyester resin composition containing from 1 to 30 parts by mass of a carboxylic acid anhydride and preferably further containing from 1 to 50 parts by mass of at least one type of a short fiber reinforcing material, a thermoplastic elastomer, or an acrylic rubber core-shell polymer per 100 parts by mass of an aliphatic polyester resin containing not less than 50 mass % of a polyglycolic acid resin, the effective thickness being 1 mm or more; a downhole tool for hydrocarbon resource recovery formed from the molded product having an effective thickness of 1 mm or more; an aliphatic polyester resin composition for the downhole tool member for hydrocarbon resource recovery; and a well drilling method. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10119359-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115322447-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11142678-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10352125-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10337279-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2688769-C1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10465468-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11428064-B2 |
priorityDate |
2014-03-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |