http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017170434-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c3d427ee590a0b2a025f92aa2e67981e |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-813 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K77-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L51-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H10K50-854 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-0268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L51-5268 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L51-56 |
filingDate | 2014-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_851ca11445a33926acc9a1b747f3f7d3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f37b825b4936d836ef060a3e87b94a0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dca5dca28005f9cc9829400d403c51f |
publicationDate | 2017-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2017170434-A1 |
titleOfInvention | Method for manufacturing substrate, substrate, method for manufacturing organic electroluminescence device, and organic electroluminescence device |
abstract | The purpose of the present invention is to reduce light, which is absorbed at an interface of an organic electroluminescence device and disappears, thereby improving the efficiency of extraction of light that is drawn to the outside. A substrate 11 is coated with polymer to form a polymer layer 12 ; ion bombardment stress resulting from plasma is applied to the polymer layer 12 to form a corrugated layer 13 having a plurality of corrugated parts; and a first electrode, an organic light-emitting layer, and a second electrode are successively formed on the substrate, on which the corrugated layer is formed, thereby manufacturing an organic electroluminescence device. In addition, a metal layer 23 may be additionally formed on the polymer layer, ion bombardment stress and thermal stress may be applied simultaneously to form corrugated parts, and the metal layer may then be removed. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10164216-B2 |
priorityDate | 2013-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23968 http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458357694 |
Total number of triples: 25.