abstract |
Polymer composition containing a) a polymer, b) a zeolite, whereby the total amount of the components a) and b) in the composition is higher than 90 wt %, in particular higher than 94 wt %, more preferred higher than 98 wt % and the total amount of water determined by TGA in the temperature range of 25 to 380° C. with a rate of 5° C./min is lower than 15 wt %, based on the amount of residuals obtained after the TGA measurement has been continued to 550° C. |