abstract |
An active material composite particle is capable of suppressing a reaction with a sulfide solid electrolyte material at high temperature. The active material composite particle may include an oxide active material of rock salt bed type and a coat layer containing lithium niobate formed on a surface of the oxide active material, wherein a thickness of the coat layer is in the range of 25 nm to 94 nm. |