http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016268600-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8643191cf8ae2c2cac1b18a99fb2c00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_df042a4ee931885669af2c40184b0ec5
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-20
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-139
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0471
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-364
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-362
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-1397
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-405
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5815
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-583
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-052
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-40
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62
filingDate 2015-12-11-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b66d474f8603bf82afa7a1b770fdcbc3
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_441853f7b44b70ffb4dbdc545a2adcac
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_135a7c8f2f3ca2b5d09a9117fbb1347d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1f6b9ffab0095bb4b80c94b19a51ce2
publicationDate 2016-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber US-2016268600-A1
titleOfInvention Method for manufacturing positive active material for all-solid lithium-sulfur battery
abstract A method for manufacturing a positive active material for an all-solid Lithium-Sulfur battery includes preparing a lithium sulfide solution by dissolving lithium sulfide in anhydrous ethanol. A mixture is prepared by mixing a carbon fiber to the lithium sulfide solution. A lithium sulfide-carbon fiber composite is prepared by drying the mixture of the carbon fiber and the lithium sulfide solution to deposit the lithium sulfide on a surface of the carbon fiber. The lithium sulfide-carbon fiber composite is heated at 400 to 600° C.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111554888-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112678780-A
priorityDate 2015-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013202961-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2011052998-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450378462
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449097739
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10290727
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID431819883
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419559581
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID2724049
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419538410
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID297
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID702

Total number of triples: 43.