Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ee33b0e3e7398cf6fc957eeee59d510 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e88b0fc56396d3980546dd6e432e23e2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-30 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G51-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-48 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G51-04 |
filingDate |
2016-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ff05a68f1b313a3655632ea76d98812 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58a4d847c0f5f14b960ce4ba2d3deb50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c3fd8d8423303fdb8d78bf67d961b73b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac2880adacc457e03b3ad7940a4864d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1a2cdae2df376e8ab5a1af438c1821d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8eb30138e04b3d23a37005d5ea403f85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d44955bc991100e38dff987168831c8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_976b26d7f6b120100305998c14cc171d |
publicationDate |
2016-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2016167979-A1 |
titleOfInvention |
Method for making spherical cobalt oxyhydroxide |
abstract |
A method for making a spherical cobalt oxyhydroxide requires a controlled crystallization reactor. A buffer agent is put into the controlled crystallization reactor. The buffer agent is capable of controlling a reacting speed of reactants. A cobalt salt solution and an alkaline solution as the reactants are added into the buffer agent in the controlled crystallization reactor. The reactants react together in a controlled crystallization method, the reactants being agitated only at a bottom region of the container of the controlled crystallization reactor. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11305243-B2 |
priorityDate |
2013-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |