Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9001cb95c9c1cbbe55f36062bf591f21 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N25-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N33-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-08 |
filingDate |
2013-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_996216d293004b9ce38a648b84d28520 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26b450270d3d7c0d0f074b4f6ecd2e6f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccf9bdbd9033ff7819d5a21822a9dea3 |
publicationDate |
2016-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2016057994-A1 |
titleOfInvention |
Aplatelet Clays for Sustained Release of Active Ingredients |
abstract |
A method of forming an active control ingredient that controls target living species over an extended period of time commences by providing a clay material that has a structure substantially depleted of platelets (“aplatelet”). The aplatelet clay material is heated with a solid active control agent to a temperature of at least about 10° C. above the melting point of the solid active control agent. The aplatelet clay material then is loaded with the heated solid active control agent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11140993-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2020093276-A1 |
priorityDate |
2013-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |