Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1c87faedd93ed22aa30b91961dff1085 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01F5-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H13-10 |
filingDate |
2013-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c6cde711f67f1ee1cd3ece21b14a986e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96901ebc1d9505957bd0a29d35be8e42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_929ebb0570eb1a686a07c5862d8fc0ae |
publicationDate |
2015-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015318078-A1 |
titleOfInvention |
Electrical insulating paper |
abstract |
An electrical insulating paper having 40-80 wt % of aramid fibrid, 10-50 wt % of aramid pulp, and 10-50 wt % of aramid short-cut. The aramid pulp is para-aramid pulp with a length of 0.5-6 mm and has a Schopper Riegler value of 15-85; the aramid fibrid is para-aramid fibrid; and the aramid short-cut is para-aramid short-cut. The paper shows a high dielectric strength and tensile index. A method for manufacturing the paper and an insulated conductor that includes the paper. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11111632-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018038984-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015376837-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9922750-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9903073-B2 |
priorityDate |
2012-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |