Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bd0cdbc5c67cf4957ed83c89140748e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2004-028 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-0402 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 |
filingDate |
2013-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_07de226bc5bb1c290a7224d90723693e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ada04b9e027573f49d6d7bfdd523d197 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_702ea7136428e029f7626891677bf352 |
publicationDate |
2015-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015311511-A1 |
titleOfInvention |
Coated nickel hydroxide powder for alkali secondary battery positive electrode active material and method of producing same |
abstract |
A coated nickel hydroxide powder that has improved dispersibility in a paste to inhibit agglomeration and can be densely packed in a three-dimensional metal porous body in the preparation of a positive electrode for alkaline secondary battery includes nickel hydroxide particles and a coating layer made of a cobalt compound and formed on a surface of the nickel hydroxide particles, wherein when 10 mL of water is added to 10 g of the coated nickel hydroxide powder to prepare a suspension, the suspension having a pH of 10.2 or higher (as measured at 25° C.). The coated nickel hydroxide powder obtained through a crystallization step and a coating step is washed in a washing step until an amount of ammonium ions eluted into a suspension obtained by adding 10 mL of water to 10 g of the coated nickel hydroxide powder becomes 0.35 mmol/L or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2021234200-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11283058-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10868292-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017077489-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10680245-B2 |
priorityDate |
2012-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |