Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_657f8fe5931a3364fda9ccca712ad398 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12458 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-12764 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B15-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-665 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-1653 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-623 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D5-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-66 |
filingDate |
2015-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c25cfd87d2d6de5f5774dd72e9ba23c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62744935352f5f5725bb6259486c5553 |
publicationDate |
2015-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015299884-A1 |
titleOfInvention |
Alloying interlayer for electroplated aluminum on aluminum alloys |
abstract |
A method of forming a coated aluminum alloy component includes first preparing the surface of the aluminum alloy component and then electrodepositing an intermediate aluminum alloy interlayer on the surface of the component from an ionic liquid. A final step includes electrodepositing an aluminum protective coating on the intermediate aluminum alloy interlayer from an ionic liquid. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108251871-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10000859-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10392948-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106782980-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2016002805-A1 |
priorityDate |
2012-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |