abstract |
A cavitation resistant polyurethane composition includes a first solution comprising a urethane prepolymer and a second solution. The urethane prepolymer is synthesized by a polymerization of about 60 to about 70 weight percent of an isocynate compound and about 30 to about 40 weight percent of a polyol. An average functional group number of the isocyanate compound is at least 2. The second solution includes about 90 to about 95 weight percent of a polyol having an average functional group number of at least 4, about 1 to about 3 weight percent of a nano-carbon, about 1 to about 3 weight percent of a colorant, about 1 to about 3 weight percent of a moisture absorbent, about 1 to about 3 weight percent of an anti-wear agent, and about 1 to about 3 weight percent of a defoaming agent. |