http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015158974-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f4a7711656877c108fcffc1b2b52cfc4 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-181 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-46 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-46 |
filingDate | 2013-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01d6fbd07ed6d16b4f0734f9e0f0a5f7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d3647eb9e282549bb7d6b01c831e938 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb20a9916e9ac32eb55c9327097c42d6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_537e8f2371356ee607a813e0da88478e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24acf47d6893ce97b297808c34ef7cac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ac8b2b1fd51d49365cdfc99a930c566 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_186c4083e1cfce3bc2f155509234b637 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cba38443e682cd21dba6b9dbc3513f2b |
publicationDate | 2015-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2015158974-A1 |
titleOfInvention | Method for preparing biodegradable aliphatic-aromatic polyester copolymer resin with improved hydrolysis resistance |
abstract | There is provided a method of preparation for a biodegradable co-polyester resin with improved hydrolysis resistance, the method including performing a primary esterification reaction between an aliphatic dihydroxy compound and an aliphatic dicarboxylic acid compound, and performing a secondary transesterification reaction with addition of an aromatic dicarboxylate after the primary esterification reaction, in which a short chain alcohol-type branching agent is added to the primary esterification reaction or to the secondary transesterification reaction. In the method of the present invention, the slow esterification reaction caused by acid is performed first and the aromatic dicarboxylate compound without acidity is added thereto, thereby efficiently controlling a non-reactant or a partial-reactant affecting an acid value of a product during the reaction, so that an acid value can be controlled and hydrolysis resistance can be improved without using an excessive amount of expensive BDO, an reaction of an excessive amount of a chain extender, or using an expensive anti-hydrolysis agent. Further, by minimizing an amount of the branching agent used herein, tear strength can be improved. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019007523-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11427677-B2 |
priorityDate | 2012-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |