Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6b4a80ac02f1ecd0e698ec665e9b36b6 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2381-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G75-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G75-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G75-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G75-16 |
filingDate |
2015-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5745f19cab04e7841e2b3e7d0fab6734 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ddd4ed47f751d6e24e6009719181072 |
publicationDate |
2015-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015152227-A1 |
titleOfInvention |
Recyclable polyarylene sulfide and preparation method thereof |
abstract |
This disclosure relates to recyclable polyarylene sulfide that may exhibit and maintain excellent mechanical properties, particularly does not exhibit decrease in melt viscosity when it is molten, and thus, exhibit little deterioration of mechanical properties, and a method for preparing the same. n The polyarylene sulfide has initial melt viscosity measured at 300□ of 300 to 6000 poise, and melt viscosity after heat treated and molten at 300□, equal to or greater than the initial melt viscosity |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9249263-B2 |
priorityDate |
2010-03-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |