http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015152209-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C1-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F236-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F136-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F136-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L11-02 |
filingDate | 2013-03-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29e713900548d94ee8888d7d725fce85 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ca4866ebe72f954370aba5e5dfd1e3db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4695fd00077e9f6b4884f5f0969ae8e3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18c5c5aa53c113c66f0ba395e1d6dfea |
publicationDate | 2015-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2015152209-A1 |
titleOfInvention | Polychloroprene latex, polychloroprene latex composition, and molded article |
abstract | An object of the present invention is to provide a polychloroprene latex with improved rubber coagulability that gives a film superior in strength by dip molding, a polychloroprene latex composition, and a molded article. The polychloroprene latex is prepared by polymerization of 2-chloro-1,3-butadiene alone or by polymerization of raw monomers at least containing 2-chloro-1,3-butadiene and 2,3-dichloro1,3-butadiene and has a precipitation rate of 5 to 40%, as calculated according to Equation (I). In Equation (I), A is the mass (g) of the dry product, which is obtained by adding 50 ml of saturated aqueous solution of calcium hydroxide at 23° C. to 50 g of a latex having a solid matter concentration adjusted to 45 to 65 mass % at a liquid temperature of 23° C. over 2 minutes, filtering and collecting the generated precipitate with a 80-mesh wire mesh, and drying the precipitate at 110° C. for 3 hours; B is the mass of the latex before the dropwise addition (50 g); and C is the solid matter concentration (mass %) of the latex before the dropwise addition. n n n n n n n n n Precipitation n n n n n n rate n n n n n n n ( n % n ) n n n = n n n A n n B n × n n C n 100 n n n n × n 100 n n n n n n ( n I n ) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10344158-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10377893-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2018112055-A1 |
priorityDate | 2012-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 98.