Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-502 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-77348 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-643 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7734 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L33-502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C30B33-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C30B33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-02 |
filingDate |
2013-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50a6c41378a46a6b1c9cbdf5750a2ce4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46ae0a4a7d1f0d334f3d2e0f72862456 |
publicationDate |
2015-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015137037-A1 |
titleOfInvention |
Method for treating surface of phosphor, phosphor, light-emitting device, and illumination device |
abstract |
Provided are a method for treating the surface of a (Sr,Ca)AlSiN 3 nitride phosphor that can improve the moisture-resistance reliability thereof without deterioration in optical properties, a phosphor, a light-emitting device, and an illumination device. The surface of a phosphor is treated in an immersion step of immersing a phosphor of which the host crystal has a crystal structure substantially identical with that of (Sr,Ca)AlSiN 3 crystal in an aqueous ammonium phosphate-containing solution (Step 1 ) and a heat-treating step of leaving the phosphor after the immersion step in an environment at a temperature of 250 to 550° C. for 2 to 24 hours (Step 2 ). |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10153405-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11773323-B2 |
priorityDate |
2012-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |