Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1eeedc82260c25045bafc3c3fa601efc |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-547 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-02167 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-2254 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-312 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-316 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-186 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-1804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-02282 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-823807 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-02118 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L21-2255 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01L31-18 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L31-18 |
filingDate |
2014-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d24ca4146c958ce8623285b8db5c3dc5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a28eb4d78a9ba47f18f98253fb7b59f6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2453bcf65014a78c8cd8e0e0791778be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f683f59faaf134f8e3f0f9ce9dcf7670 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73a49978b0e7dbd34d02604c7a9061a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b9c66ea6abaaf2dde58b90938cf8fa0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7da6c18690d8f81e5bf9b2007b0c5386 |
publicationDate |
2015-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015118786-A1 |
titleOfInvention |
Method of producing solar cell |
abstract |
A method of producing a solar cell, including: a first coating step in which a pre-wet composition is spin-coated on a surface of a semiconductor substrate; a second coating step in which a diffusing material including a solvent and a diffusing agent containing a first impurity element is spin-coated on the surface where the pre-wet composition has been spin-coated, so as to form a coating film of the diffusing agent; and a first impurity diffusion layer forming step in which the semiconductor substrate having the coating film formed thereon is heated, so as to form a first impurity diffusion layer in which the impurity element contained in the diffusing agent is diffused. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3920240-A4 |
priorityDate |
2013-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |