Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_79b5f9d76648dfc226a261cfb970de9c |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5406 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-215 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D127-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 |
filingDate |
2013-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc5dd3495b6418fb96e7537af42b64a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d12723225dfae30b4c377914a7777335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e63a92987d6e2a6195075b12aebf8cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ef3c44fe39ffe08bbdbcac8911d2d36d |
publicationDate |
2015-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2015093511-A1 |
titleOfInvention |
Method of manufacture for graphene fluoropolymer dispersion |
abstract |
A method for forming a dispersion includes mixing graphene particles, a fluorosilane coupling agent and a first solvent to produce a first dispersion wherein the graphene particles are from about 0.1 to about 0.8 weight percent of the first dispersion. The method includes concentrating the first dispersion by removing the first solvent to produce a second dispersion wherein the graphene particles are from about 2.0 to about 10.0 weight percent of the concentrated dispersion. The concentrated dispersion is mixed with a fluoropolymer dispersion including a second solvent, a surfactant, and fluoropolymer particles wherein the fluoropolymer dispersion has a solids content of about 30 weight percent to about 50 weight percent to form a second dispersion. A polymer binder in a third solvent is mixed with the second dispersion to form the coating dispersion. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107118646-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110804349-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111234696-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105969014-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115058063-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110724433-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112592626-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110724433-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111471345-A |
priorityDate |
2013-10-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |