http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2015047709-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-2059 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E10-542 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-2031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-3676 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 |
filingDate | 2013-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_60d527d4477f058d128f1330aa827827 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_daacf712b3a9f8defd5342f7bbe64570 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31d3c6351ee306fb286f9ae17acdfd68 |
publicationDate | 2015-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-2015047709-A1 |
titleOfInvention | Titanium oxide paste |
abstract | The present invention aims to provide a titanium oxide paste which is excellent in printability and which allows for production of a porous titanium oxide layer having a high porosity with a small amount of impurities on the surface thereof even by low-temperature firing, a method of producing a porous titanium oxide laminate using the titanium oxide paste, and a dye-sensitized solar cell. n The titanium oxide paste of the present invention contains titanium oxide particles, a (meth)acrylic resin, and an organic solvent. The paste has a viscosity of 15 to 50 Pa·s and a thixotropic ratio of 2 or greater. A dried mass obtained by heating the paste at a temperature-increasing rate of 10° C./min from 25° C. to 300° C. in the atmospheric environment contains 1% by weight or less of the (meth)acrylic resin and the organic solvent. |
priorityDate | 2012-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |