Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c85d78c6a4459b5dbbc49c82a4c5c107 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2265 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-22 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 |
filingDate |
2012-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d978ddf12125749080f7069f8812fcac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_039289a640fbea48de8bddb20ba61f13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b55160b01ffa4c07c63d3afb68c76ade http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecc257b2f6c238735b127d9802cc1bee |
publicationDate |
2014-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2014357776-A1 |
titleOfInvention |
Rotomolding composition |
abstract |
The instant invention provides a rotomolding composition. The a rotomolding composition comprises at least 95 percent by weight of a thermoplastic polymer; and from 0.1 to 3 percent by weight of metal oxide lamellae; wherein the rotomolding composition is characterized by at least one of the following properties: (a) having a retention at elongation at break of at least 85 percent after 4000 hours of accelerated aging; or (b) having a ductility improvement of at least 50 percent relative to a similar composition free of said metal oxide lamellae |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110760119-A |
priorityDate |
2011-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |