abstract |
The invention provides an adhesive composition for conduction between electrical elements, comprising 25 to 46 parts by weight of nitrile-butadiene rubber with Mooney viscosity ranged from 50 to 75 (ML 1+4@100)° C., 25 to 45 parts by weight of acrylic oligomer, 16 to 32 parts by weight of thermoplastic resin, two organic peroxides having different one-minute half-life temperatures from each other, and a coupling agent. The thermoplastic resin is selected from the group consisting of phenoxy resin, poly(methyl)methacrylate copolymer, polystyrene copolymer and Novolak resin. |