Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cdda975363b1e86f8f3485e16147b5cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a309595469ec63e86546d96f656fe3cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_921ade7e25c5c1b2c001d75798cab2e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95c89084d61fd47ae93470ca7c96f184 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-267 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L15-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L15-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-3085 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A01N25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L15-22 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A01N25-04 |
filingDate |
2014-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f70dd8d0bcaf13388ccc20d45765cb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ae2ee87e650e83ba5343ef41d9b6183 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac7d505449b625d0dd7b28a5a9460ddc |
publicationDate |
2014-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-2014339469-A1 |
titleOfInvention |
Biodegradable superabsorbent polymer composition with good absorption and retention properties |
abstract |
The present invention generally relates to a method for the production of a superabsorbent composition comprising the process steps:n i. production of a hydrogel by radical polymerization of an aqueous monomer solution containing at least one monomer ii. drying the hydrogel to obtain a water-absorbing polymer structure iii. surface crosslinking of the water-absorbing polymer structure to obtain a surface-crosslinked water-absorbing polymer structure, iv. incorporation of a starch compound in one or at least two of the variants V1 to V6,n V1. in process step i. into the monomer solution V2. after process step i. and prior to process step ii. into the hydrogel V3. in process step ii. V4. after process step ii. and prior to process step iii. into the water-absorbing polymer structure V5. in process step iii V6. after process step iii onto the surface-crosslinked water-absorbing polymer structure. n nn The present invention also related to a superabsorbent composition obtainable according to this method, a particulate superabsorbent composition and a composite, a sanitary article core and a sanitary item, furthermore chemical products and also the use of this superabsorbent composition in chemical products. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11680184-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112076702-A |
priorityDate |
2006-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |