A method to make a phosphorus modified zeolite can include providing a zeolite including at least one ten member ring in the structure steaming the zeolite, mixing the zeolite with one or more binders and shaping additives, and then shaping the mixture. The method can include making a ion-exchange. The shaped mixture can be steamed. Phosphorous can be introduced on the catalyst to introduce at least 0.1 wt % of phosphorus, such as be dry impregnation or chemical vapor deposition. A metal, such as calcium, can be introduced. The catalyst can be washed, calcinated, and then steamed. The steaming severity (X) can be at least about 2. The catalyst can be steamed at a temperature above 625° C., such as a temperature ranging from 700 to 800° C. The catalyst can be used in alcohol dehydration, olefin cracking, MTO processes, and alkylation of aromatics by alcohols with olefins and/or alcohols. |